TEM study of structural hardening in a new martensitic steel for aeronautic application

Abstract: A new generation of high performance martensitic steel hardened by FeNiAl intermetallic nanoprecipitates has been investigated using conventional and advanced Transmission Electron Microscopy (TEM). Cs-corrected high resolution TEM has been used to provide a fine and accurate microstructural characterization: the shape, size and crystallographic characteristics of the nanoprecipitates have been identified. TEM in situ straining tests have been performed to determine the relevant parameters, which control the d… Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1

Citation Types

0
2
0

Year Published

2018
2018
2024
2024

Publication Types

Select...
6

Relationship

0
6

Authors

Journals

citations
Cited by 7 publications
(2 citation statements)
references
References 24 publications
0
2
0
Order By: Relevance
“…It is assumed that the improved tempering resistance and therefore the increased TMF lifetime of the dual hardening alloy is caused by the combination of secondary hardening carbides and intermetallic precipitates. Upon ageing, the intermetallic particles precipitate very fast and homogeneously distributed due to their coherency to the iron matrix, expanding the preferred precipitation sites for secondary hardening carbides from dislocations and grain boundaries to interfaces between the NiAl particles and the iron matrix . This leads to an increased amount of precipitation sites, thus a more homogeneous distribution and size refinement of the secondary hardening carbides, resulting in an increased tempering resistance.…”
Section: Resultsmentioning
confidence: 99%
“…It is assumed that the improved tempering resistance and therefore the increased TMF lifetime of the dual hardening alloy is caused by the combination of secondary hardening carbides and intermetallic precipitates. Upon ageing, the intermetallic particles precipitate very fast and homogeneously distributed due to their coherency to the iron matrix, expanding the preferred precipitation sites for secondary hardening carbides from dislocations and grain boundaries to interfaces between the NiAl particles and the iron matrix . This leads to an increased amount of precipitation sites, thus a more homogeneous distribution and size refinement of the secondary hardening carbides, resulting in an increased tempering resistance.…”
Section: Resultsmentioning
confidence: 99%
“…( 10 ) denotes the self-diffusion coefficient. For iron, D 0L = 3.71 × 10 –4 m 2 s −1 , Q L = 269 kJ mol −1 31 , b = 2.5 × 10 –10 m 32 , while the shear modulus was obtained from Ref. 33 .…”
Section: Discussionmentioning
confidence: 99%