“…PVDF‐HFP composite films presented the obvious indication of the in situ formation of HImMg fillers in the PVDF‐HFP matrix. The characteristic peak with a monoclinic structure of HImMg was assigned at 2 θ = 14.1°, 14.5°, 20.6°, 23.0°, 24.7°, 25.2°, 26.8°, 28.4°, 29.1°, 29.4°, 37.4°, 41.7°, 43.2°, 44.3°, and 44.7°, as presented in Figure S2 19 . In both prepared methods, the peak intensity of diffraction angle 2 θ for HImMg fillers apparently increased with increasing filler content.…”