Template synthesis of water-dispersible and magnetically responsive carbon nano test tubes

Abstract: Water-dispersible and magneto-responsive carbon nano test tubes with a controlled length (1.3 microm) and diameter (35 nm) were synthesized by using the nanochannels of anodic aluminium oxide as a template.

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
19
0
1

Year Published

2009
2009
2015
2015

Publication Types

Select...
7
1

Relationship

0
8

Authors

Journals

citations
Cited by 31 publications
(20 citation statements)
references
References 7 publications
0
19
0
1
Order By: Relevance
“…Figure 2c shows the XRD pattern of copper phyllosilicates after calcination. 26 , chemical vapour deposition 27,28 and electrochemical template synthesis 29 . On the basis of the reported synthesis procedure 27,30 , we proposed a twostep IWI method (see Methods and Supplementary Fig.…”
Section: Resultsmentioning
confidence: 99%
“…Figure 2c shows the XRD pattern of copper phyllosilicates after calcination. 26 , chemical vapour deposition 27,28 and electrochemical template synthesis 29 . On the basis of the reported synthesis procedure 27,30 , we proposed a twostep IWI method (see Methods and Supplementary Fig.…”
Section: Resultsmentioning
confidence: 99%
“…At the same time, magnetic metal or alloy filled in the cavity of CNTs is responsive to magnetic field even after a long-term storage in water. Furthermore, the metal-filled CNTs can be water dispersible after a H 2 O 2 treatment [128].…”
Section: Electrodepositionmentioning
confidence: 99%
“…The AAO-CNTs used can be either one-side open or both-side open. Foreign matters can be loaded into the carbon-deposited AAO template by using incipient wetness impregnation [40,42,[118][119][120][121], sublimation [122][123][124][125][126][127], or electrodeposition method [41,109,[128][129][130][131]. Since only the inner surface of the AAO-CNTs is exposed, the foreign matters would be selectively filled inside the hollow cores of CNTs.…”
Section: Filling Of Aao-cntsmentioning
confidence: 99%
See 1 more Smart Citation
“…17,18 Because of these unique characteristics, CNTs synthesized by the AAO template method (AAO-CNTs) are considered to be a promising candidate for systematically investigating the confinement effects of CNTs on the nanostructures loaded inside them. There are a few reports on controlling the length and diameter of AAO-CNTs, 19,20 however, the CNTs used usually have diameters larger than 10 nm. Since the smaller the CNT diameter, the more obvious the confinement effect, it is important to obtain CNTs with even smaller diameters.…”
Section: Introductionmentioning
confidence: 99%