“…When Sr 6 Co 5 O 15 was sintered by the SPS method, the obtained sample included a compound, which was different from the compound obtained in the lower temperature region mentioned above, in addition to Sr 6 From the results, Sr 6 Co 5 O 15 tends to change to other compounds depending on the heating conditions. In addition, the thermogravimetric analysis for Sr 6 Co 5 O 15 , carried out in air, showed the weight loss of 1.5% in the temperature range of 673-1123 K, suggesting the formation of oxygen defects.…”