2022
DOI: 10.1016/j.matchar.2022.112000
|View full text |Cite
|
Sign up to set email alerts
|

The anisotropic of corrosion and tribocorrosion behaviors of Ti 15Mo alloy fabricated by selective laser melting

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

0
5
0

Year Published

2022
2022
2024
2024

Publication Types

Select...
6

Relationship

2
4

Authors

Journals

citations
Cited by 13 publications
(5 citation statements)
references
References 48 publications
0
5
0
Order By: Relevance
“…The sample shows a <001> texture orientation tends to increase with the scanning strategy changing from sample I (Figure 9a) to sample IV (Figure 9d), which is consistent with the results of Figure 8. The texture index was introduced to quantify the texture intensities [ 27 ] :Texture index =eulersapce(f (g))2dx$$\text{Texture index } = \left(\int\right)_{\text{eulersapce}} \left(\left(\right. f \textrm{ } \left(\right.…”
Section: Resultsmentioning
confidence: 99%
See 1 more Smart Citation
“…The sample shows a <001> texture orientation tends to increase with the scanning strategy changing from sample I (Figure 9a) to sample IV (Figure 9d), which is consistent with the results of Figure 8. The texture index was introduced to quantify the texture intensities [ 27 ] :Texture index =eulersapce(f (g))2dx$$\text{Texture index } = \left(\int\right)_{\text{eulersapce}} \left(\left(\right. f \textrm{ } \left(\right.…”
Section: Resultsmentioning
confidence: 99%
“…The sample shows a <001> texture orientation tends to increase with the scanning strategy changing from sample I (Figure 9a) to sample IV (Figure 9d), which is consistent with the results of . The texture index was introduced to quantify the texture intensities [27] :…”
Section: Grain Morphology and Texture Evolutionmentioning
confidence: 99%
“…Throughout the entire SLM process, a high-purity argon (Ar) atmosphere was used, ensuring that the oxygen content remained below 100 ppm. A Ti-6Al-4V plate was served as the building substrate and preheated to 393 K. Based on our previous studies, 7,16 samples were produced with the parameters as follow: a scanning speed (v) of 1100 mm/s, laser power (P) set at 175 W, a layer thickness (d) of 30 μm, and a scanning distance (h) of 30 μm. Wire cutting was utilized to separate metal specimens from the plate, followed by 30-min ultrasound washing and drying in a vacuum drying oven.…”
Section: Specimen Preparationmentioning
confidence: 99%
“…6 Besides, compared with traditional techniques, SLM presents other advantages, such as notably rapid production and cost efficiency. 7 Titanium alloys prepared using SLM technology exhibit superior mechanical properties compared to casting and forging. 8 Titanium alloy as a biocompatible metal, the mechanical properties especially fatigue resistance are very important since the implant is always subjected to cyclic loading during walking.…”
Section: Introductionmentioning
confidence: 99%