“…The lattice parameter calculated from the XRD patterns of Ce 0.8 Gd 0.2 O 2Àd was 0.5411 AE 0.0002 nm regardless the type of powder used, which is in good agreement with previous reports [10,14,15]. Moreover, the logarithmic grain conductivity (log s) of the sintered pellets was approximately À2.03 and À1.40 S/cm at 500 and 700 8C, respectively, for both the high energy-milled K-and W-powder, which cannot be achieved when the GDC phase is not formed [8,9,16].…”