Abstract:The article presents results of tests concerning the effect of heat treatment on the structure and hardness of submerged arc welded joints made in steel 7CrMoVTiB10-10 (T24). The tests revealed that the welds made of steel 7CrMoVTiB10-10 required post-weld heat treatment at a temperature 750°C. The heat treatment was performed in order to protect welded structures from cracking during transport and operation as well as to prevent the development of secondary hardness.
Set email alert for when this publication receives citations?
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.