The Effect of Melt Ultrasound Treatment on the Microstructure and Age Hardenability of Al-4 Wt Pct Cu/TiC Composite

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1

Citation Types

0
1
0

Year Published

2020
2020
2023
2023

Publication Types

Select...
4

Relationship

0
4

Authors

Journals

citations
Cited by 4 publications
(1 citation statement)
references
References 38 publications
0
1
0
Order By: Relevance
“…10 D’Brass et al. 11 reported hardness as high as 132 HV for Al-4wt%-Cu matrix composites reinforced with 7.5 wt.% TiC. In Cu composites reinforced with TiC (36.24 wt.%) the hardness was 285 HV.…”
Section: Introductionmentioning
confidence: 99%
“…10 D’Brass et al. 11 reported hardness as high as 132 HV for Al-4wt%-Cu matrix composites reinforced with 7.5 wt.% TiC. In Cu composites reinforced with TiC (36.24 wt.%) the hardness was 285 HV.…”
Section: Introductionmentioning
confidence: 99%