Abstract:Electrochemical method was employed to investigate galvanic corrosion behaviors of super13Cr and N80 couples in 5% NaCl solution at different temperature. Corrosion morphologies and products of the couples were analyzed by SEM, EDS and XRD. The results show that there existed distinct potential difference between super13Cr and N80 with different degree of corrosion in 5% NaCl solution at different temperature. N80 was accelerated to corrode as anode, however, super 13Cr was protected as cathode when their coup… Show more
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.