The effect of the oxidation temperature of UO 2 pellets on the powder properties of oxidized U 3 O 8 powders has been investigated. The powder morphology, crystalline size, and BET surface area of recycled U 3 O 8 could be modified by controlling the oxidation temperature of the UO 2 pellets. Recycled U 3 O 8 powder with a high BET surface area and a small particle size could be obtained by lowering the oxidation temperature. It was also found that this low-temperature-oxidized sinter-active U 3 O 8 powder is effective in mitigating the density drop of the UO 2 pellets when the recycled U 3 O 8 powder is added. Moreover, the recycled powder acted as a grain-size-enlarging promoter in the UO 2 pellets.