“…An even more effective approach aimed at the depression of λph consists of the introduction of a structural disorder through the substitution of Co by Fe/Co [36,37,38,39], Co/Ni [40,41] Fe/Ni [29,34,38,42,43] or Fe/Co/Ni [30,31], the substitution of Sb by Sb/Sn or Sb/Ge [36], or multiple filling of the cavity by DD (didymium) [36,38,41], Mm (mischmetal) [31,41], Ce/Yb [30], Ce/Nd [44], Ce/Yb/In [45] or by a mixture of alkaline-earths [46] with the possible addition of lanthanide elements [41,42] and elements of the IIIB group [47]. Multiple filling, in particular, was thoroughly studied [48], since it ensures a broadening of the range of phonon frequencies which can be perturbed by the rattling movement of doping ions. For this reason, when designing a multiple doping, a significant difference in the mass of the different fillers is generally recommended.…”