Thermomechanical Fatigue Performance of Lead-Free Chip Scale Package Assemblies with Fast Cure and Reworkable Capillary Flow Underfills

Abstract: In this paper, we present the results of temperature cycling test for full and partial capillary flow underfilled lead-free chip scale packages (CSPs), the tests were carried out on the basis of JEDEC standard. Two kinds of representative fast cure and reworkable underfill materials are used in this study, and CSPs without underfills were also tested for comparison. The test results show that the two underfill materials reduce the thermomechanical fatigue performance of CSP assemblies. The underfill with high … Show more

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3

Citation Types

0
3
0

Year Published

2012
2012
2023
2023

Publication Types

Select...
3
3

Relationship

1
5

Authors

Journals

citations
Cited by 8 publications
(3 citation statements)
references
References 23 publications
0
3
0
Order By: Relevance
“…However, the studies on thermal fatigue that have focused on fatigue crack propagation in underfill resins are very limited 10–12 . Furthermore, in thermal cycle tests on IC packages, it is difficult to determine where and when the crack initiated and how it propagated in underfill resins because the disconnection of solder joints was usually measured electrically 13,14 . Therefore, it is important to clarify the thermal fatigue crack growth characteristics of underfill resins to understand the failure mechanism and design reliable IC packages.…”
Section: Introductionmentioning
confidence: 99%
“…However, the studies on thermal fatigue that have focused on fatigue crack propagation in underfill resins are very limited 10–12 . Furthermore, in thermal cycle tests on IC packages, it is difficult to determine where and when the crack initiated and how it propagated in underfill resins because the disconnection of solder joints was usually measured electrically 13,14 . Therefore, it is important to clarify the thermal fatigue crack growth characteristics of underfill resins to understand the failure mechanism and design reliable IC packages.…”
Section: Introductionmentioning
confidence: 99%
“…The improvement does not seem to be as much as full capillary flow underfill but it is enough to help the package pass mechanical requirements [12][13][14][15]. However, depending on the selection of materials the thermal fatigue life may easily end up worse than that without an adhesive [15][16][17]. This is true for lead-free soldered assemblies compared to eutectic SnPb soldered assemblies.…”
Section: Introductionmentioning
confidence: 99%
“…The polymeric reinforcement approaches include full capillary flow underfill (FCFU), partial capillary flow underfill (PCFU), edge bond adhesive (EBA), and corner bond adhesive (CBA) [4][5][6][7][8][9][10][11][12][13]. Although no-flow underfill, epoxy flux, and preform underfilm technologies are available in the marketplace, high volume manufacturing (HVM) of these approaches has not been adopted due to their shortcomings [14][15][16][17].…”
Section: Introductionmentioning
confidence: 99%