2019
DOI: 10.1016/j.jallcom.2019.06.330
|View full text |Cite
|
Sign up to set email alerts
|

Time-dependent corrosion properties of Sr-modified AlSi9 alloy analyzed by electrochemical techniques

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
3
1
1

Citation Types

0
5
0

Year Published

2020
2020
2024
2024

Publication Types

Select...
6
1
1

Relationship

0
8

Authors

Journals

citations
Cited by 12 publications
(5 citation statements)
references
References 35 publications
0
5
0
Order By: Relevance
“…The strontium content of 0.048% is particularly important. According to the publication by Duygun et al [16], this measured proportion is suitable for the refinement of AlSi alloys.…”
Section: Chemical Compositionmentioning
confidence: 99%
See 1 more Smart Citation
“…The strontium content of 0.048% is particularly important. According to the publication by Duygun et al [16], this measured proportion is suitable for the refinement of AlSi alloys.…”
Section: Chemical Compositionmentioning
confidence: 99%
“…The shape of the silicon solidifying in the (residual) eutectic affects the ductility of the castings. The coarse Al-Si needles or platelets are shown in Figure 1A; they greatly reduce ductility [16]. Refining the cast structure by adding trace elements, such as strontium (see Figure 1B), leads to an improvement in the morphology of the Si particles [17].…”
Section: Introductionmentioning
confidence: 99%
“…Figure 6 reports the optical microstructure of EN AC 42100-T6 RSC at higher magnifications, showcasing both representative thinnest (4-6) and thickest (15)(16) components. The microstructure is composed of α-aluminum matrix, Al-Si eutectic (indicated by green arrows), β-Al 5 FeSi platelets (highlighted by red arrows), and π-AlFeMgSi Chinese script precipitates (denoted by yellow arrows).…”
Section: Metallographical Analysismentioning
confidence: 99%
“…Another relevant aspect is the shape of silicon in the eutectic. Please note that coarser AlSi platelets greatly reduces ductility [15,16]. It is also common knowledge that the match between refined eutectic Si and smaller SDAS implies a substantial improvement in the strength of the Al-Si alloy [17].…”
Section: Introductionmentioning
confidence: 99%
“…As a part of the main eutectic (αAl + βSi), βSi particles are cathodic with respect to the αAl matrix causing the formation of micro-galvanic couples and localized corrosion phenomena [3]. Even due the effect of βSi particles on microstructure degradation is minimal, due to its high polarization and low current density, increase of eutectic (αAl + βSi) ratio in microstructure will have deleterious effect on the alloy's microstructure [4].…”
Section: Introductionmentioning