Transformation of Polysialate Matrixes from Al‐Rich and Si‐Rich Metakaolins: Polycondensation and Physico‐Chemical Properties

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
1
1
1
1

Citation Types

2
14
0

Year Published

2011
2011
2022
2022

Publication Types

Select...
6

Relationship

3
3

Authors

Journals

citations
Cited by 7 publications
(16 citation statements)
references
References 11 publications
2
14
0
Order By: Relevance
“…KO1 specimens stabilised at 30% feldspars and fired at 1100˚C show the highest resistance (23.84 MPa). This resistance is close to that of the concrete (25 MPa) [25]- [28]. Figure 19 and Figure 20 present the compression test at 1000˚C and 1100˚C respectively.…”
Section: Compressive Strengthsupporting
confidence: 67%
See 4 more Smart Citations
“…KO1 specimens stabilised at 30% feldspars and fired at 1100˚C show the highest resistance (23.84 MPa). This resistance is close to that of the concrete (25 MPa) [25]- [28]. Figure 19 and Figure 20 present the compression test at 1000˚C and 1100˚C respectively.…”
Section: Compressive Strengthsupporting
confidence: 67%
“…After drying, the raw product is subjected to a heat treatment called bisque carried out at a temperature between 900˚C and 1230˚C. Deformation and removal of the shard during this stage are limited because of the very nature of refractory raw materials [25]- [28].…”
Section: Earthenwarementioning