“…This behavior is due to the formation and development of surface microcracks at the final stages of orientational drawing, the so-called kink bands, which are initiators of the most intense crack growth at the deformation stages preceding the sample failure [ 1 , 2 ]. For this reason, in order to correctly estimate the average values of σ , E , and strain at break ( ε b ), σ av , E av , and ε av , which are important characteristics playing a key role in choosing the most appropriate fields for material applications, the number of identical samples to be tested should be increased markedly, from the generally accepted about five [ 5 , 6 , 7 , 8 ] to some dozens, or even hundreds [ 2 , 9 , 10 , 11 , 12 , 13 , 14 , 15 , 16 , 17 , 18 , 19 , 20 , 21 , 22 ]. In this case, the statistical distributions of mechanical properties can also be analyzed, and additional information obtained, for instance, on their conformity to a certain theoretical model (e.g., Gaussian [ 23 ], Weibull’s [ 9 , 10 , 11 12 , 13 , 14 , 15 , 16 , 17 , 18 , 19 , 20 , 21 , 22 ]).…”