Understanding the enhanced removal of Bi(III) using modified crystalline antimonic acids: creation of a transitional pyrochlore-type structure and the Sb(V)-Bi(III) interaction behaviors

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
2
1

Citation Types

0
5
0

Year Published

2019
2019
2023
2023

Publication Types

Select...
7

Relationship

0
7

Authors

Journals

citations
Cited by 11 publications
(5 citation statements)
references
References 50 publications
0
5
0
Order By: Relevance
“…Polyantimonic acid was synthesized using the technique adopted from [48,49], including the oxidation of Sb(III) to Sb (IV) as the first step and hydrolysis of an obtained Sb (V) solution as the second step. Antimony (III) chloride (SbCl 3, Alfa Aesar, 99.0%, Kandel, GmbH, Germany) was used as a precursor.…”
Section: Crystalline Paa Powder Preparationmentioning
confidence: 99%
“…Polyantimonic acid was synthesized using the technique adopted from [48,49], including the oxidation of Sb(III) to Sb (IV) as the first step and hydrolysis of an obtained Sb (V) solution as the second step. Antimony (III) chloride (SbCl 3, Alfa Aesar, 99.0%, Kandel, GmbH, Germany) was used as a precursor.…”
Section: Crystalline Paa Powder Preparationmentioning
confidence: 99%
“…Here, protons are displaced along the hydrogen bonds from one water molecule (oxonium ion) to another, in certain crystallographic positions in the PAA structure. The ion exchange and electrical properties of PAA significantly depend on the synthesis approach used [22][23][24]. For instance, Yu et al [23,24] obtained super soluble amorphous antimonic acid via controlled hydrolysis of SbCl 3 that was previously oxidized to SbCl 5 ; then, using 30% of hydrogen peroxide, they performed an efficient removal of Bi(III) from the solution.…”
Section: Introductionmentioning
confidence: 99%
“…The ion exchange and electrical properties of PAA significantly depend on the synthesis approach used [22][23][24]. For instance, Yu et al [23,24] obtained super soluble amorphous antimonic acid via controlled hydrolysis of SbCl 3 that was previously oxidized to SbCl 5 ; then, using 30% of hydrogen peroxide, they performed an efficient removal of Bi(III) from the solution. Hydrated antimony pentoxide was obtained also by the research group of Klestchov et al [25,26], using the same hydrolysis technique approach.…”
Section: Introductionmentioning
confidence: 99%
“…Refl ections with odd indices extinguished and it was also observed for the undoped PAA sample [24], and indicated the dehydration of compounds and the rearrangement of the structure [23, 24,34]. In the temperature range 500-600 °C, the decomposition of compounds and the formation of two phases, one of which was Sb 2 O 4.3(4) , the other -VSbO 4 phase with the crystal structure of the rutile type (sp.…”
Section: Resultsmentioning
confidence: 94%
“…The region of deformation vibrations was less sensitive to the formation of hydrogen bonds of different strengths than the region of stretching vibrations; therefore, a shift of the bands of deformation vibrations to the low-frequency region was not observed (Fig. 1) [28,34].…”
Section: Resultsmentioning
confidence: 99%