Use of Spherical Nanoindentation Protocols to Study the Anisotropic Mechanical Response of Alpha-Beta Single Colonies in Ti–6Al–4V Alloy

Soumya Mohan,
Adam L. Pilchak,
Surya R. Kalidindi