Valence-band energy-momentum densities of amorphousSiO2by(e,2e)spectroscopy

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1
1
1

Citation Types

2
4
0

Year Published

2000
2000
2016
2016

Publication Types

Select...
8

Relationship

0
8

Authors

Journals

citations
Cited by 13 publications
(6 citation statements)
references
References 33 publications
2
4
0
Order By: Relevance
“…The antibonding states in the conduction band are separated from the valence band by a band gap with width 5.7 eV. The predicted width of the band gap is much smaller than the experimental value of 8.9 eV [49], but is consistent with other ab initio calculations which have not included any non-local corrections for the exchange correlation energy [30,50,51].…”
Section: Cu Impurity In Siosupporting
confidence: 84%
“…The antibonding states in the conduction band are separated from the valence band by a band gap with width 5.7 eV. The predicted width of the band gap is much smaller than the experimental value of 8.9 eV [49], but is consistent with other ab initio calculations which have not included any non-local corrections for the exchange correlation energy [30,50,51].…”
Section: Cu Impurity In Siosupporting
confidence: 84%
“…The angle-integrated intensity curves show two typical spectra as shown in Fig.4(b). The black curve with stronger intensity near E F is attributed to the Pt electron, and the blue curve with suppressed intensity near E F and a peak at ≈ -13 eV is attributed to the bare SiO 2 /Si substrate [23]. By integrating the spectral weight of the blue shadow area which is characteristic of SiO 2 /Si ( Fig.4(b)), the spatial map ( Fig.4(c)) shows similar shape with SiO 2 /Si in the optical image ( Fig.4(a)).…”
Section: Resultsmentioning
confidence: 99%
“…4(b). The black curve with stronger intensity near E F is attributed to the Pt electron, and the blue curve with suppressed intensity near E F and a peak at ≈ -13 eV is attributed to the bare SiO 2 /Si substrate [23]. By integrating the spectral weight of the blue shadow area which is characteristic of SiO 2 /Si (Fig.…”
Section: Methodsmentioning
confidence: 99%
“…A second discrepancy, that is also observed for all other oxides studied by EMS so far [24][25][26][27], is that the ratio between the observed intensity of the O 2p derived band relative to that of the O 2s derived band differs from the calculated one by at least a factor of two. This is obvious in figure 8.…”
Section: Momentummentioning
confidence: 81%
“…In the first place, the separation between the O 2s and O 2p parts of the valence band is larger in the experiment than predicted by the FP-LMTO method by about 2 eV. This discrepancy is not unique for V 2 O 3 , and is observed for most oxides studied by EMS [24][25][26][27]. It could be a problem related to density functional theory (DFT).…”
Section: Momentummentioning
confidence: 81%