The incorporation of geosynthetic reinforcements during the rehabilitation of flexible pavements has significantly increased due to the ability of geosynthetic reinforcements to minimize reflective cracks. However, the performance of the geosynthetic-reinforced asphalt depends on the interface bond strength between the geosynthetic and the adjacent asphalt layers. Tack coat is generally used to maintain adequate bonding between the geosynthetic-reinforced asphalt layers. This study focusses on evaluating the influence of interface bond strength on the fracture resistance of geosynthetic-reinforced asphalt utilizing a new testing approach. The fracture resistance of geosynthetic-reinforced asphalt specimens was evaluated via cross-shear testing device, while interface bond strength was evaluated using interface shear strength testing. A Performance Grade (PG) 64-22 binder was applied as a tack coat at the geosynthetic-asphalt interface at four different rates that are relative to the asphalt retention capacity of the geosynthetic reinforcement. A fiberglass geocomposite was used as geosynthetic reinforcement in this study. The results indicate a correlation between interface shear strength tests and cross-shear tests, suggesting that the optimum tack coat rate is 125% of the asphalt retention capacity of the geosynthetic reinforcement to improve the fracture resistance as well as the interface bond strength of geosynthetic-reinforced asphalt layers.
The incorporation of geosynthetic reinforcements during the rehabilitation of flexible pavements has significantly increased due to the ability of geosynthetic reinforcements to minimize reflective cracks. However, the performance of the geosynthetic-reinforced asphalt depends on the interface bond strength between the geosynthetic and the adjacent asphalt layers. Tack coat is generally used to maintain adequate bonding between the geosynthetic-reinforced asphalt layers. This study focusses on evaluating the influence of interface bond strength on the fracture resistance of geosynthetic-reinforced asphalt utilizing a new testing approach. The fracture resistance of geosynthetic-reinforced asphalt specimens was evaluated via cross-shear testing device, while interface bond strength was evaluated using interface shear strength testing. A Performance Grade (PG) 64-22 binder was applied as a tack coat at the geosynthetic-asphalt interface at four different rates that are relative to the asphalt retention capacity of the geosynthetic reinforcement. A fiberglass geocomposite was used as geosynthetic reinforcement in this study. The results indicate a correlation between interface shear strength tests and cross-shear tests, suggesting that the optimum tack coat rate is 125% of the asphalt retention capacity of the geosynthetic reinforcement to improve the fracture resistance as well as the interface bond strength of geosynthetic-reinforced asphalt layers.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2025 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.