Objectives: To compare forces versus failure and shear bond strengths, and to explore their association with the base dimensions of four currently available bondable molar tubes. Materials and Methods: Tubes were bonded to hydroxyapatite discs using a conventional lightcured adhesive and were tested to shear failure with the Instron Universal testing machine. Results were analyzed using the Kruskal-Wallis test and regression and survival analyses. Results: No statistical difference was observed between the four groups globally in terms of force to failure (P 5 .059) and bond strength (P 5 .179). However, regression analysis showed that each 1 mm 2 increase in base surface area required an additional force of 3.11 N to debond the tube. Survival analysis showed that the tube with the greatest base dimensions had the best survival with increasing force to failure. Conclusions: Although a relationship was demonstrated between force to failure and base surface area, it was not a simple one. No statistically significant relationship was found between bond strength and base surface area. (Angle Orthod. 2012;82:536-540.)