Wrinkles with a well-ordered checkerboard pattern, created using dip-coating of poly(methyl methacrylate) on a UV–ozone-treated poly(dimethylsiloxane) substrate

Help me understand this report

Search citation statements

Order By: Relevance

Paper Sections

Select...
2
1

Citation Types

2
31
0

Year Published

2013
2013
2023
2023

Publication Types

Select...
7

Relationship

3
4

Authors

Journals

citations
Cited by 30 publications
(33 citation statements)
references
References 44 publications
(62 reference statements)
2
31
0
Order By: Relevance
“…As previously reported by a few groups, the oxidized surface of a PDMS sheet is undulated when the sheet is immersed in a polar solvent . We also observed that the polar solvents listed in Table (i.e., NMP, DMF, DMSO, EPN, and DO) induced wrinkles or creases on the surface oxidized by UV‐ozone treatment.…”
Section: Resultssupporting
confidence: 82%
See 2 more Smart Citations
“…As previously reported by a few groups, the oxidized surface of a PDMS sheet is undulated when the sheet is immersed in a polar solvent . We also observed that the polar solvents listed in Table (i.e., NMP, DMF, DMSO, EPN, and DO) induced wrinkles or creases on the surface oxidized by UV‐ozone treatment.…”
Section: Resultssupporting
confidence: 82%
“…As previously reported, the wavelength of the creases (i.e., the distance between two neighboring creases) is determined by the thickness of the oxidized layer. In the case shown in Figure , the wavelength is similar to the width of the oxidized zone.…”
Section: Resultsmentioning
confidence: 70%
See 1 more Smart Citation
“…Studies on swelling-induced wrinkling using various other methods have been reported, in which various polymeric materials, such as poly(acrylamide), 30 poly(2-hydroxyethyl methacrylate), 31 polystyrene, 32 and PDMS 18,33,34 were used. The materials were swollen with water, 30,31 toluene, 32 ethanol, 18,33 or acetonitrile.…”
mentioning
confidence: 99%
“…The materials were swollen with water, 30,31 toluene, 32 ethanol, 18,33 or acetonitrile. 34 The techniques employed to obtain stiff, thin surface layers included the use of a crosslinking agent to achieve high cross-link density 30 and UV-ozone treatment. 18,[32][33][34] However, the swelling-induced wrinkling of PDMS with a surface layer hardened by treatment with concentrated sulfuric acid and nitric acid has not been studied in detail.…”
mentioning
confidence: 99%