“…2a, we see the peculiarities in the behavior of the annealed samples in the temperature ranges of 210-310°C and 400-500°C. The obtained results are in good agreement with those of [4,5]. However, in [6], on the basis of investigation of the internal friction in cobalt, these domains are defined as ~400-500 K and 500-600 K (the α → β transi tion), which differs sufficiently from the data pre sented in [1,19,20].…”