This in vitro study evaluated the fatigue strength of different ceramic materials indicated for monolithic restorations. Disc-shaped specimens were made according to ISO 6872 from five different ceramic materials: feldspathic ceramic (FC), polymer-infiltrated ceramic network (PIC), lithium disilicate glass-ceramic (LD), zirconia-reinforced lithium silicate glass-ceramic (ZLS), and high translucent tetragonal zirconia polycrystals doped by yttrium (YZ-HT). After obtaining the mean of each material (n = 5) from monotonic load-to-failure tests, specimens (n = 20) were subjected to fatigue tests (staircase method) using a biaxial flexural setup (piston-on-three-balls), to determine the fatigue strength. The parameters used for fatigue tests were: 100,000 cycles at 10 Hz, initial load of ~ 60% of mean load-to-failure, and step size of 5% of the initial load (specific for each ceramic material). Kruskal-Wallis and Bonferroni's test (α = 0.05) were used to analyze the fatigue strength data. Fatigue strength (MPa) of the materials was statistically different among each other as follows: YZ-HT (370.2 ± 38.7) > LD (175.2 ± 7.5) > ZLS (152.1 ± 7.5) > PIC (81.8 ± 3.9) > FC (50.8 ± 1.9). Thus, it can be concluded that, in terms of fatigue, high translucent polycrystalline zirconia is the best choice for monolithic restorations as it bears the highest load before cracking/fracturing.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.