Objectives To investigate the shear bond strength and microleakage of glass ionomer cement (GIC) containing silver diamine fluoride (SDF).
Materials and Methods Sound human permanent premolars were divided into the following three groups: 1) GIC (Fuji IX), 2) GICSDF-S: GIC + SDF (Saforide), and 3) GICSDF-T: GIC + SDF (Topamine). Shear bond strength (n = 14/group) was measured using a universal testing machine and compared between groups (one-way ANOVA and Tukey HSD, p < 0.05). Microleakage (n = 15/group) at enamel and dentin margins was scored using a stereomicroscope (10x) and compared between groups (Chi-square, p < 0.05).
Results There were significant differences in shear bond strength between the GIC and GICSDF-S groups and between the GIC and GICSDF-T groups. The GIC group had the lowest shear bond strength among the groups; however, there was no significant difference between the GICSDF-S and GICSDF-T groups. The microleakage test results were not significantly different between groups at the enamel margin or dentin margins. Although the GIC group demonstrated a higher dye penetration score at the enamel and dentin margins, the difference was not significant.
Conclusions Within the limitations of this study, we conclude that incorporating SDF into GIC results in higher shear bond strength while not increasing microleakage at the enamel and dentin margins.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.