The mechanical response of alginate rafts formed by mixing liquid alginate antacid medication (Gaviscon Extra Strength Liquid Antacid) with acidic solutions was investigated by deforming isolated rafts in a shear rheometer. As rafts were deformed to varying magnitudes of applied strain, rheological parameters were identified and related to the overall strength, durability, and recoverability of rafts formed at different pH (1.1-1.7) and aging conditions (0.5-4 h). Rafts formed in the lowest acidity solutions (pH 1.4, 1.7) were elastically weak ( G'₀ = 60 , 42 Pa for un-aged raft) yet maintained their elasticity during applied shear deformation to large values of strain (γc∼90%, 50%, where G'≈G″), and displayed a low-to-moderate level of elastic recovery following large-strain deformation. Rafts formed in the highest acidity solution had the greatest strength ( G'₀ = 500 Pa for un-aged raft and 21.5 kPa for rafts after 0.5 h of aging), reduced durability (γc∼2.5%, independent of aging), and displayed the greatest recoverability. A trade-off existed between un-aged raft strength and durability while recovery was dependent on durability, solution pH, and age. Rheometry-based evaluations of alginate rafts could be used for the informed design of future gastric retention and antacid products.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.