The photopolymerization of styrene in emulsion is achieved in a conventional double-wall reactor equipped with a LED ribbon coiled around the external glass wall. Styrene mixed to acridine orange is added to the water phase containing sodium dodecyl sulfate, a water-soluble N-heterocyclic carbene-borane and disulfide, and irradiated. Highly stable latexes are obtained, with particles up to a diameter of 300 nm. The ability to reach such large particle sizes via a photochemical process in a dispersed medium is due to the use of visible light: the photons in the visible range are less scattered by larger objects and thus penetrate and initiate better the polymerizations. They are also greener and cheaper to produce via LEDs, and much safer than UVs. The method presented does not require any specific glassware; it works at lower temperature and delivers larger particles compared to thermal processes at similar solids contents and surfactant concentrations.
borane. Further work will focus on further extending the scope of the Boron-based photoinitiation to longer wavelengths. ASSOCIATED CONTENT Supporting Information. Synthetic details for the preparation and characterization of NHCB 3, polymer characterizations and modeling details.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.