Amorphous iron phosphate, FePO4.2H2O, was synthesized at ambient temperature using an inorganic sol-gel method coupled with a microwave route. The experimental conditions for the gelling of the Fe (III)-H3PO4 system are defined. Potentiometric Time Titration (PTT) and Potentiometric Mass Titration (PMT) methods were used to investigate the acid-base surface chemistry of obtained phosphate. Variations of surface charge with the contact time, Q = f(t), are examined for time contact ranged from 0 to 72 hours. The concentrations suspensions used for this purpose were 0.75, 1.25, and 2.5 g/L. The point of zero charges (PZC) and isoelectric point (IEP) were defined using the derivative method examining the variations , at lower contact time. A value of 5.4 was obtained for both PZC and IEP. Q in the function of the t method is performed for synthesized FePO4. 2H2O in NaCl and KCl electrolytes. The optimal surface charge of 40 C corresponding to insertion of 4.2x10-4 M of Na+ or K+, is achieved in explored conditions. The results suggest that the synthesized iron phosphate is amorphous.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.