The no prep technique to ceramic veneer have some advantages, one of the most important is the preservation of tooth structure. Purpose: Evaluate fracture resistance in bovine teeth, of ceramic veneer in different thickness (0,3 to 1,0mm). Methods: 60 teeth were selected for this study. Forty fifth ceramic veneer were made for each tooth, variating the thickness in: G1 -0,7mm; G2 -0,5mm; G3 -0,3mm and G4 -1,0mm (control group).Flexural strength test was carried out after 24h of luting. The results were analysed by ANOVA and HSD of Tukey. Results: the results showed that was no statistic difference between the groups (G1-297.2200; G2 -294.5467; G3 -291.9380 and G4 -290.0733). Conclusion: The ceramic veneer thickness didn't have influence in the final flexural strength.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.