Consideration of the possibility of transporting compressed hydrogen through existing gas pipelines leads to the need to study the regularities of the effect of hydrogen on the mechanical properties of steels in relation to the conditions of their operation in pipelines (operating pressure range, stress state of the pipe metal, etc.). This article provides an overview of the types of influence of hydrogen on the mechanical properties of steels, including those used for the manufacture of pipelines. The effect of elastic and plastic deformations on the intensity of hydrogen saturation of steels and changes in their strength and plastic deformations is analyzed. An assessment of the potential losses of transported hydrogen through the pipeline wall as a result of diffusion has been made. The main issues that need to be solved for the development of a scientifically grounded conclusion on the possibility of using existing gas pipelines for the transportation of compressed hydrogen are outlined.
The methodology for testing pipeline steels is suggested on the assumption that for the destruction of pipes in field oil pipelines by the mechanism of grooving corrosion the simultaneous fulfillment of such conditions as the occurrence of scratches on the lower generatrix of the pipe, eventually growing into a channel in the form of a groove, emulsion enrichment with oxygen, presence of pipe wall metal in a stressed state, presence of chlorine-ion in the oil-water emulsion is required. Tests are suggested to be carried out in 3 % aqueous solution of NaCl with continuous aeration by air on bent plates 150×15×3 mm, made of the analyzed steel, the middle part of which is under the action of residual stresses σres, close to the level of maximum equivalent stresses σeqv in the wall of the oil pipeline, with the presence of a cut on this part on the inner side of the plate as an initiator of additional mechanical stresses. Using the value of the modulus of normal elasticity of the analyzed steel, the degree of residual strain of the elastic-plastic body from this material, corresponding to the value σres ≈ σeqv is calculated, based on which the plates are bent to the required deflection angle, after which the cut is applied to them. After keeping the plates in the corrosive medium for each of them the increase in depth of the cut as a result of corrosion of the walls by the corrosive medium is analyzed, from which the rate of steel K by the mechanism of grooving corrosion is calculated taking into account the duration of tests. Corrosion rate values for two pipe steel grades determined by the suggested procedure are given. The comparison of K values obtained leads to the conclusion about the higher resistance to grooving corrosion of 09G2S steel.
The paper deals with a non-destructive method of detecting hydrogenated sections of pipelines, which is based on variations of the level of mechanical stresses generated in the surface layers of the steel pipe material during its hydrogenation. The use of a magnetoanisotropic method based on the phenomenon of metal magnetoelastic anisotropy development, which consists in the variation of the magnetic properties of ferromagnetic materials in direction and magnitude under the influence of mechanical stresses, is proposed as a way to register that variation. Based on the results of tensile testing of carbon steel plates with measurement of the difference in principal mechanical stresses (DPMS) occurring in metal, as well as experiments on electrolytic hydrogenation of specimens with measurement of the DPMS signal, it was confirmed that when steel structures are saturated with hydrogen, tensile stresses are generated in the surface layers, the magnitude of which increases as the concentration of hydrogen increases in the metal. In this case, it is assumed that the indicated dependence between the hydrogen concentration in the metal and the stresses arising as a result of hydrogenation is linear. For the example of lamellar specimens made of pipe low-carbon steel, the possibility of using the magnetoanisotropic method for registering sections of underground pipelines with a high content of hydrogen is substantiated, which can become the basis for a method of diagnosing sections of pipelines with broken insulation for the possibility of their further operation. The scientific novelty of this article is the establishment of a relationship between the hydrogen content in the metal, the stresses that arise in this case, and the change in the magnetic properties of ferromagnetic materials, characterized by the magnitude of the DPMS signal. This study contributes to the understanding of the process of hydrogenation of metals, and may be useful in detecting and preventing damage to gas and oil pipelines caused by hydrogen embrittlement as a cause of stress corrosion.
The work describes the experimental definition of the main factors that contribute to the emergence of grooving corrosion: availability of abrasive particles in flow which are transported in specific terms when they are capable of scratching the bottom generating line of a pipeline by creating stress concentrators; availability of considerable residual stresses in pipe metal; oxygen availability in reaction zone.
The production, transportation, and storage of liquefied natural gas (LNG) is a promising area in the gas industry due to a number of the fuel’s advantages, such as its high energy intensity indicators, its reduced storage volume compared to natural gas in the gas-air state, and it ecological efficiency. However, LNG storage systems feature a number of disadvantages, among which is the boil-off gas (BOG) recovery from an LNG tank by flaring it or discharging it to the atmosphere. Previous attempts to boil-off gas recovery using compressors, in turn, feature such disadvantages as large capital investments and operating costs, as well as low reliability rates. The authors of this article suggest a technical solution to this problem that consists in using a gas ejector for boil-off gas recovery. Natural gas from a high-pressure gas pipeline is proposed as a working fluid entraining the boil-off gas. The implementation of this method was carried out according to the developed algorithm. The proposed technical solution reduced capital costs (by approximately 170 times), metal consumption (by approximately 100 times), and power consumption (by approximately 55 kW), and improved the reliability of the system compared to a compressor unit. The sample calculation of a gas ejector for the boil-off gas recovery from an LNG tank with a capacity of 300 m3 shows that the ejector makes it possible to increase the boil-off gas pressure in the system by up to 1.13 MPa, which makes it possible to not use the first-stage compressor unit for the compression of excess vapours.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.