Post annealing treatment is generally needed for additively manufactured titanium alloy to decompose metastable phases, alleviate residual stress, and improve ductility. In this work, in-situ electrical resistivity and line profile analysis of X-ray diffraction were utilized for monitoring phase transformation behaviors and dislocation evolutions of a laser powder bed fusion-built Ti-6Al-4V alloy under post annealing treatment. Besides, hardness and tensile tests were adopted for revealing the effects of phase transformation and dislocation evolutions on the mechanical properties. The results indicated that post annealing treatment decomposed martensitic α′ into lamellar α + β and eliminated dislocations efficiently. The martensite decomposition rate increased with the annealing temperature. Annealing at 700 °C for 4 h eliminated 98% of the dislocations, and further annealing has only a limited influence on the dislocation density. Annealing at 700 °C for 16 h is beneficial for achieving a high ductility of 10.3% owing to the favorable equilibrium lamellar α + β microstructure. These findings provide valuable insights for optimizing post annealing treatment procedures to enhance the mechanical properties of additively manufactured Ti-6Al-4V alloys.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.