Ultrananocrystalline diamond (UNCD) films with up to 0.2% total nitrogen content were synthesized by a microwave plasma-enhanced chemical-vapor-deposition method using a CH4(1%)/Ar gas mixture and 1%–20% nitrogen gas added. The electrical conductivity of the nitrogen-doped UNCD films increases by five orders of magnitude (up to 143 Ω−1 cm−1) with increasing nitrogen content. Conductivity and Hall measurements made as a function of film temperature down to 4.2 K indicate that these films have the highest n-type conductivity and carrier concentration demonstrated for phase-pure diamond thin films. Grain-boundary conduction is proposed to explain the remarkable transport properties of these films.
The transport properties of diamond thin films are well known to be sensitive to the sp2/sp3-bonded carbon ratio, the presence of the grain boundaries and other defects, and to the presence of various impurities. In order to clarify the roles these factors play in the conduction mechanisms of nitrogen-doped ultrananocrystalline diamond (UNCD), Raman scattering, near edge x-ray absorption fine structure (NEXAFS), soft x-ray fluorescence (SXF), and secondary ion mass spectroscopy (SIMS) measurements were performed. Transmission electron microscopy analysis of nitrogen doped UNCD has previously indicated that the films are composed of crystalline diamond nano-grains with boundaries of amorphous carbon, and NEXAFS measurements reveal that the global amount of sp2-bonded carbon in these films increases slightly with nitrogen doping. The nitrogen content is quantified with high-resolution SIMS analysis, while NEXAFS and SXF indicates that the nitrogen exists primarily in tetrahedrally coordinated sites. These measurements indicate that the overall grain boundary volume of nitrogen-doped ultrananocrystalline diamond is increasing, while the grains themselves remain pure diamond. This supports our previously reported hypothesis that grain boundary conduction is the mechanism for the observed increase in conductivity in ultrananocrystalline diamond with nitrogen doping.
Ultrananocrystalline diamond (UNCD) films were prepared by microwave plasma chemical vapor deposition using argon-rich Ar∕CH4 plasmas at substrate temperatures from ∼400 to 800°C. Different seeding processes were employed to enhance the initial nucleation density for UNCD growth to about 1011sites∕cm2. High-resolution transmission electron microscopy, near-edge x-ray absorption fine structure, visible and ultraviolet Raman spectroscopy, and scanning electron microscopy were used to study the bonding structure as a function of growth temperature. The results showed that the growth of UNCD films is much less dependent on substrate temperature than for hydrogen-based CH4∕H2 plasmas. UNCD with nearly the same nanoscale structure as those characteristic of high-temperature deposition can be grown at temperatures as low as 400°C with growth rates of about 0.2μm∕hr. The average grain size increased to about 8nm from 3 to 5nm that is characteristic of high-temperature growth, but the relative amounts of sp3 and sp2 bonding remained unchanged. These results suggest that the activation energy for UNCD growth is about 2–3Kcal∕mole compared with ∼28kcal∕mole for traditional growth chemistries, and that hydrogen plays an important role in the growth of UNCD films using hydrogen-poor plasmas.
Ultrananocrystalline diamond film deposition by direct-current plasma assisted chemical vapor deposition using hydrogen-rich precursor gas in the absence of the positive column
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.