We present a systematic analysis of the iron loss behavior of grain oriented silicon steels containing different Si contents using transmission electron microscopy. When the silicon content changed in the range of 3-6.5 wt%, the iron loss showed a convex profile and the maximum iron loss was observed in 5.2 wt% silicon steel. This maximum iron loss should be ascribed to the formation of antiphase boundaries that acted as pinning centers in the magnetic domain wall.KEY WORDS: grain oriented silicon steel; iron loss; anti-phase boundary; magnetic domain wall.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.