All tested zirconia showed similar VHN, and the monolithic zirconia had similar roughness compared to one of the conventional zirconias. In addition, the monolithic zirconia showed similar flexural strength and Weibull modulus compared to the others even though its mean grain size was larger. The total transmittance of monolithic zirconia was higher than only one of the conventional zirconias tested.
This study evaluated microstructural and crystallographic phase changes after grinding (G) and regeneration firing/anneling (R) of Y-TZP ceramics. Thirty five bars (Lava TM and Ice Zirkon) were divided: Y-TZP pre-sintered, control (C), regeneration firing (R), dry grinding (DG), dry grinding+regeneration firing (DGR), wet grinding (WG) and wet grinding+regeneration firing (WGR). Grinding was conducted using a diamond bur and annealing at 1,000°C. The microstructure was analyzed by SEM and the crystalline phases by X-ray diffraction (XRD). XRD showed that pre-sintered specimens contained tetragonal and monoclinic phases, while groups C and R showed tetragonal, cubic and monoclinic phases. After grinding, the cubic phase was eliminated in all groups. Annealing (DGR and WGR) resulted in only tetragonal phase. SEM showed semi-circular cracks after grinding and homogenization of particles after annealing. After grinding, surfaces show tetragonal and monoclinic phases and R can be assumed to be necessary prior to porcelain layering when grinding is performed.
Grinding with a diamond stone partially transformed the crystalline phase on the surface of a Y-TZP ceramic from tetragonal to monoclinic zirconia while simultaneously increasing the surface roughness and wettability. The t-m transformation could be reversed by heat treatment at 800°C or 900°C for 60 minutes or 1000°C for 30 minutes.
Introduction: The Y-TZP zirconia used for prosthetic infrastructure, in some clinical situations, can be exposed to the oral environment. In these situations, a polished surface without changes is extremely important. Objective: The aim of this study was to evaluate the mean roughness (Ra) and Vickers hardness of Y-TZP zirconia (Lava™) after simulating ten years of brushing. Material and method: Thirty-six Y-TZP bar-shaped specimens (20mm X 4mm X 1.2mm) were divided into three groups: storage in distilled water (DW, n=12, control); brushing with distilled water (BDW, n=12) and brushing with distilled water and fluoride toothpaste (BFT, n=12). Brushing was performed using a brushing machine with a soft-bristled toothbrush, simulating 10 years of brushing (878.400 cycles, 100gf). The mean roughness (Ra in μm) and Vickers hardness (VHN) of all specimens were measured twice: before and after the experimental treatment, in profilometer and microhardness tester (500gf, 30 seconds), respectively. Data were analyzed using the two-way ANOVA test (α = 0.05). Result: The interaction between groups was not significant for roughness (p = 0.701) nor for hardness (p = 0.928). The final averages for Ra (μm) were equal to: DW - 0.63; BDW - 0.64; and, BFT - 0.68. The final averages for Vickers hardness (VHN) were: DW - 1301.16; BDW - 1316.60; and, BFT - 1299.58. Conclusion: It was concluded that the brushing with distilled or fluoridated toothpaste was not able to change the roughness and hardness of Y-TZP zirconia used in this study.
Brushing Y-TZP with conventional dentifrice increased roughness, while brushing with whitening dentifrice reduced roughness. Neither dentifrice changed the crystallographic phases after brushing.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.