A technological clayey sandstone sample from Wadi Qena locality, Eastern Desert of Egypt, was directed to processing. Fine kaolin and clean silica sand were produced after intensive attrition scrubbing of the sample. To increase the quality of the produced silica, it was subjected to reverse anionic flotation to minimize its iron content. In this respect, conventional flotation tests using three anionic oxyhydryl surfactants namely: sodium dodecyl benzene sulphonate, sodium naphtha sulphonate, and sodium dodecyl sulphate, were tried. Results showed a privilege action for sodium dodecyl sulphate to remove most of the iron oxide content of the sample. A statistical Box-Behnken design was constructed to optimize the process efficiency. It was shown that from a flotation feed contained 360 ppm Fe 2 O 3 and 1190 ppm Al 2 O 3 , sand concentrate contained 29 ppm Fe 2 O 3 and 564 ppm Al 2 O 3 , was produced. The optimum flotation conditions were 3.86 kg/t sodium dodecyl sulphate dose, 3.22 flotation pulp pH, 1226 rpm impeller speed, and 22.24 L/min airflow rate. Variables interaction effects results showed that flotation separation efficiency was significantly influenced by air flow rate and cell impeller speed of the process.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.