This work aims to evaluate the effects of feldspar substitution by basalt on porcelain tile composition with respect to its porosity, flexural strength, and pyroplastic deformation. Three ceramic formulations with different amounts of feldspar substituted with basalt, 50% (C1), 75% (C2), and 100% (C3), were evaluated at three different temperatures, 1200, 1220, and 1240 °C. Specifically, the effect of replacing feldspar with basalt on the pyroplastic deformation of ceramic bodies was analysed using optical fleximetry. The porosity of C1 at 1200 °C was 19.3 ± 2.9%, while that of composition C3 was 22.2 ± 0.7% at 1240 °C. The flexural strength was strongly influenced by the temperature. For C1 at 1200 and 1240 °C, flexural strengths of 11.1 ± 0.6 and 22.2 ± 1.9 MPa, respectively, were obtained. Regarding fleximetry, thermal deformation decreased with an increase in the amount of feldspar substituted with basalt. It was observed that C2 and C3 deformed less at high temperatures than the other combinations of compositions and temperature, probably owing to the lower amount of residual glass phase present during cooling. Compositions with higher substitution amounts of basalt (i.e., C2 and C3) exhibited more stable thermal behaviour than C0.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.