A porcine calvaria defect study was carried out to investigate the bone repair potential of three-dimensional (3D)-printed poly-ε-caprolactone (PCL) scaffolds embedded with nanoporous PCL. A microscopic grid network was created by rapid prototyping making a 3D-fused deposition model (FDM-PCL). Afterward, the FDM-PCL scaffolds were infused with a mixture of PCL, water, and 1,4-dioxane and underwent a thermal-induced phase separation (TIPS) followed by lyophilization. The TIPS process lead to a nanoporous structure shielded by the printed microstructure (NSP-PCL). Sixteen Landrace pigs were divided into two groups with 8 and 12 weeks follow-up, respectively. A total of six nonpenetrating holes were drilled in the calvaria of each animal. The size of the cylindrical defects was h 10 mm and Ø 10 mm. The defects were distributed randomly using following groups: (a) NSP-PCL scaffold, (b) FDM-PCL scaffold, (c) autograft, (d) empty defect, (a1) NSP-PCL scaffold + autologous mononuclear cells, and (a2) NSP-PCL scaffold + bone morphogenetic protein 2. Bone volume to total volume was analyzed using microcomputed tomography (µCT) and histomorphometry. The µCT and histological data showed significantly less bone formation in the NSP-PCL scaffolds in all three variations after both 8 and 12 weeks compared to all other groups. The positive autograft control had significantly higher new bone formation compared to all other groups except the FDM-PCL when analyzed using histomorphometry. The NSP-PCL scaffolds were heavily infiltrated with foreign body giant cells suggesting an inflammatory response and perhaps active resorption of the scaffold material. The unmodified FDM-PCL scaffold showed good osteoconductivity and osseointegration after both 8 and 12 weeks.
We tested the hypothesis that erythropoietin (EPO) enhances bone formation after posterolateral spinal fusion (PLF) in a rabbit model. Thirty-four adult rabbits underwent posterolateral intertransverse arthrodesis at the L5-L6 level using 2.0 g autograft per side. The animals were randomly divided into two groups receiving subcutaneous daily injections of either EPO or saline for 20 days. Treatment commenced 2 days preoperatively. Hemoglobin was monitored at baseline and 2, 4, and 6 weeks after fusion surgery. After euthanasia 6 weeks postoperatively, manual palpation, radiographic, and histomorphometric examinations were performed. Bone volume of the fusion mass was estimated by CT after 6 weeks. EPO increased bone fusion volume to 3.85 ccm (3.66-4.05) compared with 3.26 ccm (2.97-3.55) in the control group (p < 0.01). EPO treatment improved vascularization of the fusion mass and increased hemoglobin levels (p < 0.01). Fusion rate tended to be higher in the EPO group based on manual palpation, CT, and radiographic examinations. For the first time EPO has shown to augment bone formation after autograft PLF in a rabbit model. Increased vascularization provides a partial explanation for the efficacy of EPO as a bone autograft enhancer.
Stem cell and hydrogel therapy is able to partly regenerate IDD and maintain perfusion and permeability of the vertebral endplate and subchondral bone. Dynamic contrast-enhanced MRI may become an important tool in future investigation of the vertebral endplate.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.