This paper investigated the production of alumina from Nawan kaolin by acid leaching with sulfuric and hydrochloric acids. Kaolin was calcined at 850°C and was leached with 6 M acid at 90°C, 5M NaOH followed by HCl solutions were added to the leaching liquor, and the precipitated aluminum hydroxide was converted to alumina by calcination at 900°C. Materials were characterized by FTIR, XRD, and SEM techniques. The alumina extraction percent was determined at different leaching times (30-180 min) and solid/liquid ratios (0.05-0.15 g/ml). The purity of kaolin is about 95%. The percent of extraction of alumina rapidly increases with the solid/liquid ratio up to 0.1 g/ml then decreases thereafter. The percent of extraction of alumina is higher for HCl than H2SO4. The size of the chloride and sulfate ions is the key factor that controls the percent of extraction of alumina from calcined kaolin under the studied conditions.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.