By studying the minority carrier lifetime in recently manufactured commercially available n‐ and p‐type float‐zone (FZ) silicon from five leading suppliers, we observe a very large reduction in the bulk lifetime when FZ silicon is heat‐treated in the range 450–700 °C. Photoluminescence imaging of these samples at the wafer scale revealed concentric circular patterns, with higher recombination occurring in the centre, and far less around the periphery. Deep level transient spectroscopy measurements indicate the presence of recombination active defects, including a dominant center with an energy level at ∼Ev + 0.5 eV. Upon annealing FZ silicon at temperatures >1000 °C in oxygen, the lifetime is completely recovered, whereby the defects vanish and do not reappear upon subsequent annealing at 500 °C. We conclude that the heat‐treatments at >1000 °C result in total annihilation of the recombination active defects. Without such high temperature treatments, the minority carrier lifetime in FZ silicon is unstable and will affect the development of high efficiency (>24%) solar cells and surface passivation studies.
(2016) Permanent annihilation of thermally activated defects which limit the lifetime of float-zone silicon. Physica Status Solidi A .
Permanent WRAP URL:
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.