Iron ore sintering is an important source of "dioxins", polychlorinated dibenzo-p-dioxins and dibenzofurans (PCDD/Fs). This paper reports on attempts to identify materials, conditions, and mechanisms responsible for PCDD/F formation (i) by investigating salient properties of ores (viz., with respect to oxidation, condensation, and chlorination of model organics) and (ii) by mimicking the industrial process on a microscale with real-life materials. Principles of Design of Experiments (DOE) are employed. The reactivities of iron ores differ greatly. Limonite/goethite "soft" ore is a very active oxidation catalyst (e.g., for benzene and phenol), a property that may be useful in cleaning up crude sintering process offgases, whereas hematite/magnetite "hard" ore is not. The latter, however strongly promotes condensation of phenol to dibenzofuran. A newly built lab-microscale sintering facility could satisfactorily imitate the large-scale process, in part or as a whole. Results obtained with realistic feed mixtures point at dioxin formation in the sinter bed at levels significant enough to explain a major part of the outputs observed in the real-life process. With approximately 8 ppm (wt) of chloride added as NaCl, the PCDD/F output doubled, but with the same proportion of chlorine administered as C2Cl4, the dioxin output was over 2 orders of magnitude larger. The use of process reverts, etc. containing chlorinated organics should therefore be avoided. PCDD/F congener patterns are also reported and compared with those observed in practice.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.