Thin films of zinc oxide (ZnO) with ammonia solution to 300ml of aqueous solution Zn(NO3)2 . 6H2O (0.3M) are created via (CBD) technique on commercial glass substrates with bath temperature (80± 5) °C and annealing temperatures at (373, 473 and 573)K at constant time of 1h. The deposited films optical absorbance was defined utilizing SP3000NANO optima (UV-V is spectrophotometer) and shows that the optical energies gaps for ZnO films increase slightly through a rise in temperature of annealing of the samples at 373K and 473K and register around 3.77eV and 3.78eV respectively. While the energy gap decreases to 3.73eV with increase the annealing temperature at 573K. The wide band gap ZnO has applications of wide array in areas include solar cells, light conductors, chemical sensors and ultraviolet laser diodes.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.