Hypereutectic AI-Si alloys with minor additions of Sr were directionally solidified with a temperature gradient of 125°Ccm 1 in the liquid. Silicon in the range 14-17 wt%, Sr in the range 0.0-0.5 wt% and specimen traction velocities between 1 and 1500#msec -1 were used. The relationship between hardness and traction velocity and spacing in eutectic silicon morphologies is defined and shown to be of the same form as that for yield stress. The possibility of using hardness measurements to indicate mechanical properties is discussed. The complex regular silicon structure makes a significant contribution to the hardness of hypereutectic alloys. This makes the relationship between hardness and traction velocity more complex adding difficulties to the use of hardness to measure mechanical properties.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.