Vibratory cavitation erosion tests were carried out on as-cast NiAl intermetallic compounds containing 46.5 to 62.1 at. pct Ni. The erosion rate decreased with increasing nickel content by over two orders of magnitude, from a high of 16.4 to 0.11 mg⅐h Ϫ1 . These low erosion rates exhibited by the nickel-rich alloys containing 58 and 62.1 at. pct Ni, the interruptions in their mass loss with time, and the unusual effects associated with surface finish and intensity of cavitation were found to be associated with the stress-induced martensitic transformation. Alloys containing 58 to 62 at. pct Ni have the potential for use as materials for the cavitation protection of hydraulic machinery.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.