In this study, effect of types and replacement ratio of alkali activator on compressive strength of ground granulated blast furnace slag mortar has been reviewed. Types of alkali activator are NaOH, Ca(OH)2, Na2SO4, and KOH. Replacement ratio of alkali activator is 7.5, 10, 12.5, and 15%, respectively. As results, under high temperature curing condition, 1 day compressive strength development with NaOH and KOH was higher than that of Ca(OH)2 and Na2SO4. Regardless of types of alkali activator, compressive strength increased with increasing pH. This can be explained by the fact that impermeable film on the surface of slag which is generated when slag contacts water has been destroyed by alkali activator, and this promotes hydration reaction. Also, 1 day age compressive strength of specimen with high temperature curing was higher than that of specimen with standard curing. 28 days age compressive strength of specimen with high temperature curing was less than or equal to that of specimen with standard curing.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.