Before loading, the percentages of continuous margins in dentin were superior (p<0.05) for groups C and D (71.1% and 87.2%, respectively) compared to groups A and B (55.7% and 48.3%, respectively). After loading, group D (79.8%) was statistically superior in dentin compared to all of the other groups (43.6%, 35.9%, and 54.4%, respectively). In occlusal enamel, no significant difference was found between groups. The percentage of enamel fractures and the percentage of noncontinuous margins in proximal enamel were high, with no significant difference between liners. It can be concluded that for the materials used in this study, a 1-mm-thick lining with an extremely low elastic modulus (2-3 GPa) could redistribute shrinkage stress. The use of a flowable composite did not significantly improve MA.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.