The formation of biofilm on denture bases is a recurrent clinical problem that favors the development of denture stomatitis. The effectiveness of a hygiene protocol in a 3D-printed denture base resin is still uncertain. Objective To evaluate of the effectiveness of immersion, associated or not with brushing in a soap solution, on the biofilm control of a 3D-printed denture base resin. Methodology Specimens of denture base resins [Cosmos Denture (COS) and Classico (CLA/control)] were contaminated in vitro with Candida albicans and immersed in sodium hypochlorite 0.25% (SH, alkaline peroxide) AP, chlorhexidine digluconate 2% (CD or PBS-Control), associated or not with brushing with 0.78% Lifebuoy soap. Roughness was evaluated before and after brushing and immersion. The effectiveness of the protocols was assessed by CFU/mL, cellular metabolism (XTT), scanning electron microscopy (SEM), and confocal scanning laser microscopy. Data were analyzed by T student, ANOVA/Welch, and Tukey/Gomes–Howell pos-hoc tests (α = 0.05). Results CLA showed greater roughness than COS. CFU/mL and XTT were higher in COS resin with a higher hyphae formation. Immersion in SH and CD eliminated CFU/mL and reduced XTT for both resins, associated or not with brushing. AP reduced CFU/mL only when associated with brushing. Conclusions The biofilm on the 3D-printed resin was thicker and presumably more pathogenic, regardless of its smoother surface. Immersions in SH 0.25% and CD 2% are effective hygiene protocols for both resins, associated or not with brushing. AP should be recommended when associated with brushing with a Lifebuoy 0.78% solution.
The aim of this study was to evaluate the bond strength between two types of artificial teeth with a 3D-printed denture base resin using different bonding agents. Materials and methods: Two types of artificial teeth were evaluated: 3D-printed (Cosmos TEMP) and prefabricated polymethylmethacrylate (Biotone) bonded to cylinders (2.5 mm in height and 5 mm in diameter) of 3D-printed denture bases (Cosmos Den-
PurposeTo evaluate the effect of immersion in disinfecting solutions on the color stability of denture base resins and artificial teeth obtained by 3D printing.Materials and methodsForty discs (15 × 3 mm) were obtained for each group: Lucitone 550 and Cosmos Denture 3D (denture base resins), Duralay and Cosmos TEMP 3D (artificial teeth resins). The discs were immersed in disinfectant solutions: Corega Tabs, 2% chlorhexidine digluconate, 0.25% sodium hypochlorite, and distilled water. Color measurements were obtained with a spectrophotometer before immersion in disinfectants and after the simulated periods of 6 and 12 months. Data (ΔE00) were submitted to mixed three‐way ANOVA and Bonferroni post‐test.ResultsFor denture base resins, Cosmos Denture 3D showed greater color change regardless of the solution and immersion time. The immersion time of 6 months influenced the color change of the denture base resins regardless of the disinfectant solution. For the artificial teeth resins, the immersion time of 12 months showed a significant color change when compared to 6 months. Cosmos TEMP 3D showed greater color change for all solutions, except for 0.25% sodium hypochlorite. Duralay resin showed greater color change in 2% chlorhexidine, regardless of immersion time.ConclusionsFor denture base resins, the immersion time significantly changed the color regardless of the solution. For artificial teeth resins, Cosmos TEMP 3D showed greater color changes in all solutions when compared to Duralay, except for 0.25% sodium hypochlorite. Chlorhexidine digluconate significantly changed the color of Duralay.
PURPOSE The aim of this study was to evaluate the flexural strength of a 3D-printed denture base resin (Cosmos Denture), after different immediate repair techniques with surface treatments and thermocycling. MATERIALS AND METHODS Rectangular 3D-printed denture base resin (Cosmos Denture) specimens (N = 130) were thermocycled (5,000 cycles, 5℃ and 55℃) before and after the different repair techniques (n = 10 per group) using an autopolymerized acrylic resin (Jet, J) or a hard relining resin (Soft Confort, SC), and different surface treatments: Jet resin monomer for 180 s (MMA), blasting with aluminum oxide (JAT) or erbium: yttrium-aluminum-garnet laser (L). The control group were intact specimens. A three-point flexural strength test was performed, and data (MPa) were analyzed by ANOVA and Games-Howell post hoc test (α = 0.05). Each failure was observed and classified through stereomicroscope images and the surface treatments were viewed by scanning electron microscope (SEM). RESULTS Control group showed the highest mean of flexural strength, statistically different from the other groups ( P < .001), followed by MMA+J group. The groups with L treatment were statistically similar to the MMA groups ( P > .05). The JAT+J group was better than the SC and JAT+SC groups ( P < .05), but similar to the other groups ( P > .05). Adhesive failures were most observed in JAT groups, especially when repaired with SC. The SEM images showed surface changes for all treatments, except JAT alone. CONCLUSION Denture bases fabricated with 3D-printed resin should be preferably repaired with MMA+J. SC and JAT+SC showed the worst results. Blasting impaired the adhesion of the SC resin.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.