Objective: Biodegradable polymers can replace damaged tissue components using tissue engineering techniques. The objective of this study is to determine an optimum environment for polymer scaffolds to improve the proliferation of fibroblast cells capable of wound repair. Method: In this study, the addition of polysaccharides, such as chitosan (CH) or hyaluronic acid (HA), to a polyurethane (PU) polymer was evaluated using different methods to determine if they affect scaffold morphology and cell activity of fibroblasts prepared from human foreskin tissues. Mechanical properties, such as tensile strength, contact angle and swelling test, were used to check the physical and mechanical properties of the scaffold. Fibroblast growth was also measured at 24, 48 and 72 hours. Results: Scanning electron microscopy (SEM) determined that a 3:1 ratio of PU/CH scaffold, developed by electrospinning, allowed the formation of a uniform structure in scaffold fibres. Physical mechanical tests showed that PU electrospun scaffolds were not modified by the addition of CH. The mean stretch and mean water absorption increased significantly using the PU/CH scaffold, compared with the PU scaffold. However, the mean tensile strength and the mean contact angle, used to study space and porosity, did not differ between scaffolds. Fourier transform infrared spectroscopy confirmed the functional groups (–OH, –NH and –C=O) in the PU/CH scaffold, compared with PU or CH chemical structures alone. HA was then added to CH and PU/CH scaffolds to evaluate the growth of fibroblast cells. Results showed that cell viability and the number of cells, using MTT and trypan blue exclusion assay, respectively, increased significantly at 24, 48 and 72 hours of culture in PU/CH/HA scaffold compared to HA, CH/HA, and PU/HA. Moreover, PU/HA at 48 and 72 hours also increased cell viability and cell numbers compared to HA and CH/HA scaffolds. However, scaffolds at 72 hours had limited space for cell growth. Moreover, SEM data demonstrated that fibroblasts were able to proliferate, penetrate, migrate and survive on PU/HA and PU/CH/HA three-dimensional scaffolds, especially during the first 48 hours. Furthermore, 4′,6-diamidino-2-phenylindole (DAPI) staining confirmed that fibroblasts could penetrate PU scaffolds and showed higher cell viability and lower cellular damage in PU/CH/HA, compared to CH/HA and PU/HA scaffolds. Finally, flow cytometry using CD90 and CD105 surface markers revealed that >90% of cells isolated from the human dermis were fibroblasts. Conclusion: In summary, PU/HA and PU/CH/HA scaffolds were found to be biocompatible and provided a suitable environment for the growth and proliferation of fibroblasts, which filled and covered all pores between the fibres. The new scaffold used in this study, made of synthetic and natural polymers, is a good candidate for applications in tissue engineering. It is therefore recommended to use PU in grafts or in wound dressing.
Introduction: Recently, the application of nanofibrous mats for dressing skin wounds has received great attention. In this study, we aimed to fabricate and characterize an electrospun nanofibrous mat containing polycaprolactone (PCL), chitosan (CTS), and propolis for use as a tissue-engineered skin substitute. Methods: Raw propolis was extracted, and its phenolic and flavonoid contents were measured. The physiochemical and biological properties of the fabricated mats, including PCL, PCL/CTS, and PCL/CTS/Propolis were evaluated by scanning electron microscopy (SEM), atomic force microscopy (AFM), mechanical analysis, swelling and degradation behaviors, contact angle measurement, cell attachment, DAPI staining, and MTT assay. On the other hand, the drug release pattern of propolis from the PCL/CTS/Propolis scaffold was determined. A deep second-degree burn wound model was induced in rats to investigate wound healing using macroscopical and histopathological evaluations. Results: The results revealed that the propolis extract contained high amounts of phenolic and flavonoid compounds. The fabricated scaffold had suitable physicochemical and mechanical properties. Uniform, bead-free, and well-branched fibers were observed in SEM images of mats. AFM analysis indicated that the addition of CTS and propolis to PCL elevated the surface roughness. MTT results revealed that the electrospun PCL/CTS/Propolis mat was biocompatible. The presence of fibroblast cells on the PCL/CTS/Propolis mats was confirmed by DAPI staining and SEM images. Also, propolis was sustainably released from the PCL/CTS/Propolis mat. The animal study revealed that addition of propolis significantly improved wound healing. Conclusion: The nanofibrous PCL/CTS/Propolis mat can be applied as a tissue-engineered skin substitute for healing cutaneous wounds, such as burn wounds.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.