Charcoal is the residual waste from the heat decomposition process of carbon-containing materials, most of whose components are carbon. This study aims to determine the frequency of charcoal water as an electrolyte solution to produce an alternative energy source that is environmentally friendly. The method used in the experiment is to find the type of water with the addition of zinc and copper and to measure the sample voltage of charcoal water to determine the optimum mass and optimum interaction time. The variation in the volume of water with 50 ml and 100 ml of charcoal water was produced, with the addition of zinc and copper in the size of 1x5 cm, 2x5 cm, 3x5 cm which resulted in fluctuations in each data. For example, the difference in voltage value in the type of water used is tap water, 100 ml well water with the addition of zinc and copper measuring 2x5 cm. Tap water, namely with an electric voltage of 0.65 V, 0.70 V, 0.60 V, 0.60 V, 0.75 V and well water with an electric voltage of 0.60 V, 0.55 V, 0.55 V, 0.55 V, 0.55 V. Less than the maximum frequency produced with two glasses that are not made into a series or parallel circuit.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.
customersupport@researchsolutions.com
10624 S. Eastern Ave., Ste. A-614
Henderson, NV 89052, USA
This site is protected by reCAPTCHA and the Google Privacy Policy and Terms of Service apply.
Copyright © 2024 scite LLC. All rights reserved.
Made with 💙 for researchers
Part of the Research Solutions Family.