Ferritic/martensitic oxide dispersion strengthened steel with a nominal composition of Fe-9Cr-2W-0.2Ti-0.12C-0.35Y 2 O 3 was produced by mechanical alloying in a high energy horizontal Simoloyer attritor. Powder samples were collected at intervals of 0.5, 1, 2, 3, 5, 7 and 10 h and analysed by X-ray diffraction, scanning electron microscopy, energy-dispersive spectroscopy, transmission electron microscopy and differential thermal analysis. The alloying elements (Cr and W) got dissolved in the matrix in 7 h milled powder. Crystallite size decreased rapidly with milling time up to 5 h milling and reached a stable size of ∼12 nm after 7 h, whereas strain and lattice parameter were found to increase with milling time. The particle size increased up to 2 h milling and then decreased with milling time. A fine and uniform particle size of ∼25 nm was obtained after 7 h milling. The alloying process and distribution of alloying elements/Y 2 O 3 is studied in the present work.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.