TARIK AYDOG MUŞ, EL _ IF TARHAN BOR, and ŞAK _ IR BOR Porous TiNi alloys with porosities in the range of 51 to 73 pct were prepared successfully applying a new powder metallurgy fabrication route in which magnesium was used as a space holder, resulting in either single austenite phase or a mixture of austenite and martensite phases dictated by the composition of the starting powders, but entirely free from secondary brittle intermetallics, oxides, nitrides, and carbonitrides. Since transformation temperatures are very sensitive to composition, deformation, and oxidation, for the first time, transformation temperatures of porous TiNi alloys were investigated using chemically homogeneous specimens in as-sintered and aged conditions eliminating secondary phase, contamination, and deformation effects. It was found that the porosity content of the foams has no influence on the phase transformation temperatures both in as-sintered and aged conditions, while deformation, oxidation, and aging treatment are severely influential.
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.