The adsorption properties of Ukrainian Transcarpathian clinoptilolite in aqueous copper(H) solutions under dynamic conditions have been investigated. Under optimum conditions (pH of Cu2+ solution = 7.1; adsorbent thermally modified at 120-170°C for 2.5 h; flow rate of Cu2+ solution through adsorbent = 3 ml/min), the adsorption capacity of the clinoptilolite towards copper amounted to 725 ng/g. The conditions for the desorption of copper(II) from clinoptilolite have been studied. Of the desorbents tested, the best were HNO3 (1:1) and HNO3 (1:2) solutions. Their effectiveness in extracting copper(II) ions under the desorption conditions employed amounted to 100%.
The adsorption properties of Ukrainian Transcarpathian mordenite in aqueous copper(II) solutions under dynamic conditions have been investigated. Under optimum conditions (pH of Cu2+ solution = 6.5; adsorbent thermallly modified over 2.5 h at 150°C; rate of passage of Cu2+ solution through adsorbent = 3 ml/min) the adsorption capacity of the mordenite towards copper amounted to 1020 μg/g. Copper is effectively desorbed by an aqueous solution of HNO3 (1:2). Under optimum desorption conditions the effective extraction of copper was 99.8%.
BackgroundIn spite of the fact that terbium is one of the rarest elements in the Earth’s crust, it is frequently used for the production of high technological materials. At the result, an effective combination of sample preparation procedure and detection method for terbium ions in different matrices is highly required. The solid-phase extraction procedure with natural Transcarpathian clinoptilolite thermally activated at 350 °C was used to preconcentrate trace amounts of terbium ions in aqueous solutions for a final spectrophotometric determination with arsenazo III.ResultsThermogravimetric investigations confirmed the existence of relations between changes that appeared during dehydratation of calcined zeolite and its sorption affinity. Since the maximum of sorption capacity towards terbium was observed at pH 8.25, a borate buffer medium (2.5 · 10−4 М) was used to maintain ionic force and solution acidity. Terbium was quantitatively removed from the solid-phase extraction column with a 1.0 M solution of sodium chloride (pH 2.5). The linearity of the proposed method was evaluated in the range of 2.5-200 ng · mL−1 with detection limit 0.75 ng · mL−1.ConclusionsDue to acceptable recoveries (93.3–102.0 %) and RSD values (6–7.1) from spiked tap water, the developed method can be successfully applied for the determination of trace amounts of terbium ions in the presence of major components of water.Graphical abstractSorption of terbium(III) ions on clinoptilolite
scite is a Brooklyn-based organization that helps researchers better discover and understand research articles through Smart Citations–citations that display the context of the citation and describe whether the article provides supporting or contrasting evidence. scite is used by students and researchers from around the world and is funded in part by the National Science Foundation and the National Institute on Drug Abuse of the National Institutes of Health.